dc.description.abstractCrack initiation and propagation process of fatigue test in semicircular notched plates at elevated temperature were conducted under strain-controlled condition in order to study the crack initiation/propagation/coalescence process and load decrease in structure having stress concentration. Test specimens made of SUS304 stainless steel are tested at 550°C and the geometry of the semicircular notched plate specimens are changed by diameter size of the circular notch in both of single-notched specimens and double-notched specimens. Photographs in all cycles were recorded to investigate crack initiation/propagation/coalescence as a function of number of applied cycle. The typical crack process is predicted by using the simplified method, namely, stress redistribution locus method as well as Neuber’s formula.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleCrack Initiation Process for Semicircular Notched Plate in Fatigue Test at Elevated Temperature
dc.typeJournal Paper
dc.journal.volume133
dc.journal.issue3
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4002539
dc.journal.fristpage31403
dc.identifier.eissn1528-8978
dc.keywordsTemperature
dc.keywordsStress
dc.keywordsFracture (Materials)
dc.keywordsCycles
dc.keywordsFatigue testing AND Stress concentration
dc.treeJournal of Pressure Vessel Technology:;2011:;volume( 133 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record