dc.description.abstractThis paper presents failure investigation on reheater pendent SA213-T22 tubes through visual inspections, steam-side scale and tube wall thickness measurements, metallurgical examinations, and creep analysis. The investigations were carried out following subsequent tube failures of the reheater pendent region of a boiler unit. Interaction event of significant internal scale formation causing the higher metal temperature and external scale exfoliation as a result of high-temperature corrosion is identified to cause the failure of the reheater pendent tube. Prevention actions are recommended to avoid similar failures in the future.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleFailure Investigation on Reheater Pendent Tubes Due to External Scale Exfoliation and Internal Scale Formation
dc.typeJournal Paper
dc.journal.volume133
dc.journal.issue6
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.4004561
dc.journal.fristpage61402
dc.identifier.eissn1528-8978
dc.keywordsCreep
dc.keywordsTemperature
dc.keywordsMetals
dc.keywordsIncrustations
dc.keywordsCorrosion
dc.keywordsFailure
dc.keywordsSteam
dc.keywordsWall thickness
dc.keywordsHigh temperature
dc.keywordsRupture
dc.keywordsThickness
dc.keywordsMeasurement
dc.keywordsBoilers AND Inspection
dc.treeJournal of Pressure Vessel Technology:;2011:;volume( 133 ):;issue: 006