    Stress Intensity Factors of Various Surface Cracks Inside a Hollow Cylinder Under Steady State Thermal Striping

    Thumbnail
    View/Open
    JPVTAS-28510#031208_1.pdf (439.3Kb)
    Date
    2009
    Author
    Toshiyuki Meshii
    Kentaro Shibata
    Metadata
    Show full item record
    Abstract
    A thermal stress problem of a long hollow cylinder was considered in this paper. The outer surface of the cylinder was adiabatically insulated, and the inner surface was heated axisymmetrically by a fluid with sinusoidal temperature fluctuations (hereafter called as thermal striping), whose temperature amplitude (ΔT) and angular velocity (ω) were constant. The heat transfer coefficient h was also assumed to be constant. The stress intensity factor (SIF) due to the thermal stress for a given cylinder configuration varies not only with these three parameters ΔT, ω, and h, but also with time. The temperature and, as a result, SIF fluctuation amplitude soon became constant (, and , 2004, “Stress Intensity Factor of a Circumferential Crack in a Thick-Walled Cylinder Under Thermal Striping,” ASME J. Pressure Vessel Technol., 126(2), pp. 157–162), which hereafter is called as steady state. If one is interested in fatigue crack growth (assuming Paris law) under this thermal stress, because the SIF range soon converges to a constant, it seemed important to know the maximum value of the steady state SIF range for a given cylinder configuration, for all possible combinations of ΔT, ω, and h. This maximum SIF evaluation is time consuming. Thus in this paper, this maximum steady state SIF range for four typical surface cracks’ deepest point, inside a hollow cylinder for all possible combinations of ΔT, ω, and h were presented as a first step. Thin-to thick-walled cylinders in the range of mean radius to wall thickness parameter rm/W=10.5–1 were considered. Crack configurations considered were 360 deg continuous circumferential, radial, semi-elliptical in the circumferential and radial directions. Normalized crack depth for all cases was in the range of a/W=0.1–0.5. In case of semi-elliptical crack, the normalized crack length a/c was all in the range of 0.063–1.
    URI
    http://yetl.yabesh.ir/yetl/handle/yetl/141795
    Collections
    • Journal of Pressure Vessel Technology

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV
     

     

    Browse

    All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV