    Failure Analysis of a 9–12%Cr Steel Superheater Tube

    Thumbnail
    View/Open
    JPVTAS-28522#061401_1.pdf (1.430Mb)
    Date
    2009
    Author
    E. Pour saeidi
    M. Aieneravaie
    M. R. Mohammadi Arhani
    Metadata
    Show full item record
    Abstract
    The failure analysis of 9–12% chromium steel tubes, containing about 2.5% molybdenum, is discussed in the present study. The component is used in a steam power plant boiler as a high-temperature superheater tube and has been in service for about 100,000 h. The failure occurred without appreciable wall thinning. Specimens were taken from the region beneath the fracture surface and investigated by optical and electron microscopes. The microstructure was composed of ferrite and grain boundary particulate carbides. The results indicated that the fracture was initiated because of the bending of the tube near the anchor and propagation of the crack through the interfaces between massive carbides and matrix (sensitized zone). Final fracture has occurred as a result of an overload due to the decreasing of load carrying section produced by crack propagation.
    URI
    http://yetl.yabesh.ir/yetl/handle/yetl/141731
    Collections
    • Journal of Pressure Vessel Technology

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV
     

     

    Browse

    All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV