dc.description.abstractAerospace aluminum alloy forgings can have the residual stresses arising from heat treatment reduced by modification to the quench cooling rates and subsequent aging treatments. A series of propeller hubs usually made from the alloy 2014 have been closed die forged from the less quench sensitive alloy 7050. These forgings have been subjected to various quenching and aging treatments in an attempt to improve the balance of mechanical properties with the residual stress magnitudes. These forgings were not amenable to stress relieving by cold compression or stretching. Warm water (60°C) and boiling water quenches are investigated in addition to quenching into molten salt (200°C) and uphill quenching from −196°C. Various dual aging treatments including retrogression and reaging have been evaluated in an attempt to optimize low residual stress magnitudes with mechanical properties. Residual stresses determined by the center hole-drilling strain-gauge method are reported in addition to electrical conductivity, stress corrosion cracking, fracture toughness, initiation fatigue, and tensile mechanical property variations. It was found that quenching into boiling water and salt at 200°C did substantially reduce the residual stress but had only a small detrimental effect on the majority of the properties measured. However, the influence of quench rate on fracture toughness was much more significant. This is attributed to both coarse grain boundary precipitation and heterogeneous precipitation of η on Al3Zr dispersoids within the grains, which promotes easier crack propagation.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleReducing Residual Stress in 7050 Aluminum Alloy Die Forgings by Heat Treatment
dc.typeJournal Paper
dc.journal.volume130
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.2931150
dc.journal.fristpage31003
dc.identifier.eissn1528-8889
dc.keywordsStress
dc.keywordsHeat treating (Metalworking)
dc.keywordsForgings (Products)
dc.keywordsQuenching (Metalworking)
dc.keywordsWater
dc.keywordsForging
dc.keywordsFracture toughness
dc.keywordsBoiling
dc.keywordsAluminum alloys
dc.keywordsTemperature measurement
dc.keywordsTemperature
dc.keywordsStress corrosion cracking AND Testing
dc.treeJournal of Engineering Materials and Technology:;2008:;volume( 130 ):;issue: 003
dc.contenttypeFulltext