dc.description.abstractA method of predicting the leak/rupture criteria for API 5L X80 and X100 line pipes was evaluated based on the results of hydrostatic full-scale tests for X60, X65, X80, and X100 line pipes with an axially through-wall (TW) notch. The TW notch test results defined the leak/rupture criteria, that is, the relationship between the initial notch lengths and the maximum hoop stresses during the TW notch tests. The defined leak/rupture criteria were then compared to the prediction of the Charpy V-notch (CVN) absorbed energy-based equation, which has been proposed by Kiefner, Maxey et al. This comparison revealed that the CVN-based equation was not applicable to the pipes having both a CVN energy greater than 120 or 130 J and flow stress greater than the level of X65. In order to predict the leak/rupture criteria for these line pipes, the static absorbed energy for ductile cracking, (Cvs)i, was introduced as representing the fracture toughness of a pipe material. The (Cvs)i value was determined from the microscopic observation of the cut and polished Charpy V-notch specimens after static three-point bending tests. The CVN energy in the original CVN-based equation was replaced by an equivalent CVN energy, (Cv)eq, which was defined as follows: (Cv)eq=4.5(Cvs)i. The leak/rupture criteria for the X80 and X100 line pipes with higher CVN energies were reasonably predicted by the modified equation using the (Cvs)i value.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleModified Equation To Predict Leak/Rupture Criteria For Axially Through-Wall Notched X80 and X100 Linepipes Having a Higher Charpy Energy
dc.typeJournal Paper
dc.journal.volume128
dc.journal.issue4
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.2349570
dc.journal.fristpage572
dc.journal.lastpage580
dc.identifier.eissn1528-8978
dc.keywordsStress
dc.keywordsPipes
dc.keywordsEquations
dc.keywordsRupture
dc.keywordsLeakage
dc.keywordsFlow (Dynamics) AND Ductile fracture
dc.treeJournal of Pressure Vessel Technology:;2006:;volume( 128 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record