dc.description.abstractA manufacturing procedure for enhancing residual stresses and thereby improving fatigue lifetime and fracture resistance of pressure vessels is proposed. The procedure involves initial autofrettage; one or more “heat soak plus autofrettage” sequences and an optional final heat soak. Stresses are calculated numerically for traditional, single autofrettage and compared with those created by the new procedure. The loss of bore compressive hoop stress due to Bauschinger effect is predicted to be significantly reduced. Associated fatigue lifetime calculations indicate that life may be improved by a factor of between 2 and 30, depending upon tube geometry and the ratio of cyclic pressure to yield strength. Repeated overload plus heat soak cycles may also be of benefit in other engineering design scenarios.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleA Re-Autofrettage Procedure for Mitigation of Bauschinger Effect in Thick Cylinders
dc.typeJournal Paper
dc.journal.volume126
dc.journal.issue4
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.1806446
dc.journal.fristpage451
dc.journal.lastpage454
dc.identifier.eissn1528-8978
dc.keywordsHeat
dc.keywordsStress
dc.keywordsAutofrettage
dc.keywordsPressure vessels
dc.keywordsFatigue
dc.keywordsSteel
dc.keywordsResidual stresses
dc.keywordsPressure
dc.keywordsCylinders AND Yield strength
dc.treeJournal of Pressure Vessel Technology:;2004:;volume( 126 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail
This item appears in the following Collection(s)

Show simple item record