dc.description.abstractFatigue crack propagation properties of welded joints were investigated on steel plate for boilers and other pressure vessels. The fatigue crack propagation properties at 300°C became similar to those at room temperature when the thermal stress could be reduced down to −1 MPa by using center cracked type specimen with longitudinal slits and a specially designed furnace. The tensile residual stress was +152 MPa in the as-welded joint, and +12 MPa after PWHT. The fatigue threshold was about 2.7, 5.1 and 7.3 MN/m3/2 for weld metal in the as-welded condition, after PWHT and the base metal, respectively.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleFatigue Crack Propagation Properties of Welded Joints at 300°C
dc.typeJournal Paper
dc.journal.volume125
dc.journal.issue2
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.1563628
dc.journal.fristpage131
dc.journal.lastpage135
dc.identifier.eissn1528-8978
dc.keywordsTemperature
dc.keywordsStress
dc.keywordsWelded joints
dc.keywordsFatigue cracks
dc.keywordsThermal stresses
dc.keywordsSteel
dc.keywordsBase metals AND Metals
dc.treeJournal of Pressure Vessel Technology:;2003:;volume( 125 ):;issue: 002
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record