Show simple item record

dc.contributor.authorP. R. Sreenivasan
dc.contributor.authorG. Bandyopadhyay
dc.contributor.authorC. G. Shastry
dc.contributor.authorM. D. Mathew
dc.contributor.authorK. Bhanu Sankara Rao
dc.contributor.authorS. L. Mannan
dc.date.accessioned2017-05-09T00:10:24Z
dc.date.available2017-05-09T00:10:24Z
dc.date.copyrightApril, 2003
dc.date.issued2003
dc.identifier.issn0094-4289
dc.identifier.otherJEMTA8-27045#227_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/128508
dc.description.abstractResidual life analysis of power plant components like boiler tubes, superheater outlet headers, reheater headers, steam pipes, etc., is important for life extension and avoidance of catastrophic failure. In this context, fracture toughness is very important. The fracture characteristics after prolonged exposure to high temperatures and pressures are likely to be different from that of the virgin material. 2.25Cr-1Mo reheater header pipe exposed at 813 K for 120,000 h was studied by instrumented impact tests (IIT) to evaluate dynamic fracture toughness and Charpy transition properties. The methods presented in this paper for estimating dynamic fracture toughness from IIT of Charpy specimens give reliably conservative results without the need for precracking. For estimating fracture appearance transition temperature (FATT) from IIT load-time traces, the equation for percent shear fracture, PSF3, gives the best 1:1 correlation with measured values from fracture surfaces. The lower bound equation for variation of fracture toughness with temperature derived in the present study is higher than that obtained from the FATT master curve (FATT-MC) approach. Comparison of Charpy indices like FATT and upper-shelf energy for the service exposed steel to results for the virgin material reported in the literature and the compositional J-Factor estimates for temper-embrittlement susceptibility indicate that the present steel, even after 120,000 h exposure to high temperature service, has probably undergone only very little or nil degradation in toughness properties.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleDynamic Fracture Toughness and Charpy Transition Properties of a Service-Exposed 2.25Cr-1Mo Reheater Header Pipe
dc.typeJournal Paper
dc.journal.volume125
dc.journal.issue2
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.1543969
dc.journal.fristpage227
dc.journal.lastpage233
dc.identifier.eissn1528-8889
dc.keywordsTemperature
dc.keywordsSteel
dc.keywordsStress
dc.keywordsFracture (Process)
dc.keywordsPipes
dc.keywordsEquations
dc.keywordsFracture toughness
dc.keywordsImpact testing
dc.keywordsFailure
dc.keywordsPhase transition temperature
dc.keywordsShear (Mechanics) AND Fracture (Materials)
dc.treeJournal of Engineering Materials and Technology:;2003:;volume( 125 ):;issue: 002
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record