dc.description.abstractIt is shown that, under certain conditions, simultaneous improvement of vibration damping capacity and interlaminar fracture toughness in composite laminates can be achieved by using polymeric interleaves between the composite laminae. The specific case of Mode II interlaminar fracture toughness and flexural damping capacity of interleaved composite laminates is studied. Graphite/epoxy, E-glass/epoxy and E-glass/polyetherimide composite laminates with polymeric interleaves of several different thicknesses and materials were tested using both the end notch flexure (ENF) test for Mode II fracture toughness and the impulse-frequency response test for flexural damping capacity. The Mode II energy release rate GIIc for all three composites increased linearly with increasing interleaf thickness up to a critical thickness, then dropped off with further increases in thickness. The damping loss factor η for all three composites increased linearly with increasing interleaf thickness up to the maximum thickness. Analytical models for predicting the influence of interleaves on GIIc and η are developed, along with a hypothesis for the critical thickness effect with regard to fracture toughness.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleImprovement of Vibration Damping Capacity and Fracture Toughness in Composite Laminates by the Use of Polymeric Interleaves
dc.typeJournal Paper
dc.journal.volume123
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.1370385
dc.journal.fristpage309
dc.journal.lastpage314
dc.identifier.eissn1528-8889
dc.keywordsLaminates
dc.keywordsEpoxy adhesives
dc.keywordsDamping
dc.keywordsVibration
dc.keywordsFracture toughness
dc.keywordsComposite materials
dc.keywordsThickness
dc.keywordsGraphite AND Glass
dc.treeJournal of Engineering Materials and Technology:;2001:;volume( 123 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record