| dc.contributor.author | Levi de O. Bueno | |
| dc.contributor.author | Flavio A. S. Serra | |
| dc.contributor.author | Fernando T. Gazini | |
| dc.contributor.author | Luiz Marino | |
| dc.date.accessioned | 2017-05-09T00:02:32Z | |
| dc.date.available | 2017-05-09T00:02:32Z | |
| dc.date.copyright | July, 2000 | |
| dc.date.issued | 2000 | |
| dc.identifier.issn | 0094-4289 | |
| dc.identifier.other | JEMTA8-27009#269_1.pdf | |
| dc.identifier.uri | http://yetl.yabesh.ir/yetl/handle/yetl/123753 | |
| dc.description.abstract | During a shutdown for general maintenance of a catalytic cracking unit, intergranular cracks were observed to occur during welding of the regenerator’s standpipe component manufactured from 2 1/4 Cr-1Mo steel. The cracking was observed to be related to intensive carbide precipitation in grain boundaries. To overcome the problem it was decided to heat-treat the relevant section of the component to dissolve these carbides and make possible its welding to a new virgin section of the tube. Samples of the material in its various conditions (virgin, ex-service, heat-treated, and welded) were taken to check the efficiency of the thermal treatment in reducing the embattlement effects and to carry out a general assessment of the remaining life of the component related to creep behavior considering notched bar creep specimens. [S0094-4289(00)00503-X] | |
| dc.publisher | The American Society of Mechanical Engineers (ASME) | |
| dc.title | Structural Integrity of a Standpipe Component in a Petrochemical Catalytic Cracking Unit: Part 2—Assessment of Embrittlement Effects | |
| dc.type | Journal Paper | |
| dc.journal.volume | 122 | |
| dc.journal.issue | 3 | |
| dc.journal.title | Journal of Engineering Materials and Technology | |
| dc.identifier.doi | 10.1115/1.482812 | |
| dc.journal.fristpage | 269 | |
| dc.journal.lastpage | 272 | |
| dc.identifier.eissn | 1528-8889 | |
| dc.keywords | Creep | |
| dc.keywords | Heat | |
| dc.keywords | Steel | |
| dc.keywords | Grain boundaries | |
| dc.keywords | Fracture (Process) | |
| dc.keywords | Embrittlement | |
| dc.keywords | Petrochemicals | |
| dc.keywords | Temperature | |
| dc.keywords | Precipitation AND Welding | |
| dc.tree | Journal of Engineering Materials and Technology:;2000:;volume( 122 ):;issue: 003 | |
| dc.contenttype | Fulltext | |