| dc.contributor.author | M. Higuchi | |
| dc.contributor.author | T. Yamauchi | |
| dc.contributor.author | Y. Tanaka | |
| dc.contributor.author | K. Iida | |
| dc.date.accessioned | 2017-05-09T00:00:42Z | |
| dc.date.available | 2017-05-09T00:00:42Z | |
| dc.date.copyright | May, 1999 | |
| dc.date.issued | 1999 | |
| dc.identifier.issn | 0094-9930 | |
| dc.identifier.other | JPVTAS-28391#196_1.pdf | |
| dc.identifier.uri | http://yetl.yabesh.ir/yetl/handle/yetl/122743 | |
| dc.description.abstract | The procedure for making crack starter weld deposit on drop-weight test (DWT) specimens was altered from two passes to one pass in about 1990. The effects of some parameters of crack starter weld process on drop-weight test results were studied. Results of this study indicated that length of overlap of the second pass and height of crack starter beads were most effective on nil-ductility temperature (T NDT ). When overlap length and bead height of two-pass deposit were small enough, T NDT obtained by two-pass deposit became lower than one-pass T NDT , the discrepancy being by as much as 25°C. T NDT values for 24 Japanese steels were determined using two different DWT methods, one-pass deposit and two-pass deposit having small overlap length and bead height. The difference of T NDT depending on DWT method could be seen only for high-toughness low-alloy steel base metals. For other materials (i.e., low-to-medium-toughness low-alloy steel base metals, weld metals, and high-toughness carbon steels), T NDT S by two-pass and one-pass deposits were essentially the same. For lower-toughness steels, T NDT was frequently lower than the temperature of v T cv − 33°C), and thus, the reference nil-ductility temperature RT NDT was determined from Charpy impact test results. These results can be taken as a way of interpreting the past toughness evaluations made for operating plants using the two-pass T NDT . | |
| dc.publisher | The American Society of Mechanical Engineers (ASME) | |
| dc.title | Effects of Crack Starter Bead Preparation in Drop-Weight Test on Nil-Ductility Transition Temperature | |
| dc.type | Journal Paper | |
| dc.journal.volume | 121 | |
| dc.journal.issue | 2 | |
| dc.journal.title | Journal of Pressure Vessel Technology | |
| dc.identifier.doi | 10.1115/1.2883686 | |
| dc.journal.fristpage | 196 | |
| dc.journal.lastpage | 202 | |
| dc.identifier.eissn | 1528-8978 | |
| dc.keywords | Weight (Mass) | |
| dc.keywords | Drops | |
| dc.keywords | Phase transition temperature | |
| dc.keywords | Ductility | |
| dc.keywords | Fracture (Materials) | |
| dc.keywords | Steel | |
| dc.keywords | Toughness | |
| dc.keywords | Discrete wavelet transforms | |
| dc.keywords | Temperature | |
| dc.keywords | Base metals | |
| dc.keywords | Alloys | |
| dc.keywords | Impact testing | |
| dc.keywords | Industrial plants | |
| dc.keywords | Metals AND Carbon | |
| dc.tree | Journal of Pressure Vessel Technology:;1999:;volume( 121 ):;issue: 002 | |
| dc.contenttype | Fulltext | |