dc.description.abstractThe objective of this investigation was to evaluate the efficacy of different weld repair techniques as applied to service-aged 2-1/4Cr-1Mo steel weldments. A header which had been in service for 244,000 h at 1050°F (565°C) was utilized for the study. Three girth welds were partially excavated and subjected to repairs using gas tungsten arc welding (GTAW), shielded metal arc welding (SMAW) with postweld heat treatment (PWHT), and without postweld heat treatment using a temperbead technique. Results show that all the weld repairs improved the creep rupture lives of the ex-service weldments and that remaining lives of several decades could be achieved in the repaired condition. The SMAW-temperbead repairs resulted in increase of rupture life, tensile strength, and impact toughness compared to the SMAW-PWHT repairs. The GTAW-PWHT repairs also produced a superior combination of mechanical properties. Remaining creep rupture lives were a function of the extrapolation procedure and specimen size. These results are described here and discussed in comparison with results previously reported for a less severely degraded condition of the steel in order to delineate the effect of prior degradation on weld repair performance.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleWeld Repair of 2-1/4Cr-1Mo Service-Aged Header Welds
dc.typeJournal Paper
dc.journal.volume121
dc.journal.issue4
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.2883713
dc.journal.fristpage345
dc.journal.lastpage352
dc.identifier.eissn1528-8978
dc.keywordsMaintenance
dc.keywordsWelded joints
dc.keywordsRupture
dc.keywordsGas tungsten arc welding
dc.keywordsSteel
dc.keywordsHeat treating (Metalworking)
dc.keywordsCreep
dc.keywordsMetals
dc.keywordsArc welding
dc.keywordsMechanical properties
dc.keywordsTensile strength AND Toughness
dc.treeJournal of Pressure Vessel Technology:;1999:;volume( 121 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record