dc.description.abstractCorrosion fatigue crack propagation tests were conducted on a high-sulfur ASTM A302-B plate steel overlaid with weld-deposited Alloy EN82H cladding. The specimens featured semi-elliptical surface cracks penetrating approximately 6.3 mm of cladding into the underlying steel. The initial crack sizes were relatively large with surface lengths of 22.8–27.3 mm, and depths of 10.5–14.1 mm. The experiments were initiated in a quasi-stagnant low-oxygen (O2 < 10 pph) aqueous environment at 243°C, under loading conditions (ΔK, R , cyclic frequency) conducive to environmentally assisted cracking (EAC) under quasi-stagnant conditions. Following fatigue testing under quasi-stagnant conditions where EAC was observed, the specimens were then fatigue tested under conditions where active water flow of either 1.7 m/s or 4.7 m/s was applied parallel to the crack. Earlier experiments on unclad surface-cracked specimens of the same steel exhibited EAC under quasi-stagnant conditions, but water flow rates at 1.7 m/s and 5.0 m/s parallel to the crack mitigated EAC. In the present experiments on clad specimens, water flow at approximately the same as the lower of these velocities did not mitigate EAC, and a free stream velocity approximately the same as the higher of these velocities resulted in sluggish mitigation of EAC. The lack of robust EAC mitigation was attributed to the greater crack surface roughness in the cladding interfering with flow induced within the crack cavity. An analysis employing the computational fluid dynamics code, FIDAP, confirmed that frictional forces associated with the cladding crack surface roughness reduced the interaction between the free stream and the crack cavity.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleCorrosion Fatigue Crack Growth in Clad Low-Alloy Steels—Part II: Water Flow Rate Effects in High-Sulfur Plate Steel
dc.typeJournal Paper
dc.journal.volume119
dc.journal.issue3
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.2842302
dc.journal.fristpage255
dc.journal.lastpage263
dc.identifier.eissn1528-8978
dc.keywordsFlow (Dynamics)
dc.keywordsAlloys
dc.keywordsSteel
dc.keywordsCorrosion
dc.keywordsFatigue cracks
dc.keywordsSulfur
dc.keywordsWater
dc.keywordsFracture (Materials)
dc.keywordsCladding systems (Building)
dc.keywordsSurface roughness
dc.keywordsCavities
dc.keywordsForce
dc.keywordsFatigue testing
dc.keywordsOxygen
dc.keywordsASTM International
dc.keywordsSurface cracks
dc.keywordsFatigue
dc.keywordsComputational fluid dynamics AND Fracture (Process)
dc.treeJournal of Pressure Vessel Technology:;1997:;volume( 119 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record