Show simple item record

dc.contributor.authorR. Viswanathan
dc.contributor.authorD. Gandy
dc.contributor.authorS. Findlan
dc.date.accessioned2017-05-08T23:54:27Z
dc.date.available2017-05-08T23:54:27Z
dc.date.copyrightNovember, 1997
dc.date.issued1997
dc.identifier.issn0094-9930
dc.identifier.otherJPVTAS-28380#414_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/119227
dc.description.abstractThis paper discusses the results of evaluations performed on service-aged piping using both conventional postweld heat treatments and temperbead repair techniques. The two repair weldments were accomplished on two 2-1/4Cr-1Mo pipe girth weldments which were removed from a utility hot reheat piping system in the fall of 1992 after 161,000 h of operation at 1000°F (538°C). Each repair was performed around one-half of the diameter of a pipe girth weldment, while the remaining half of the girth weldment was left in the service-aged condition. Post-repair metallurgical and mechanical test results indicated that both weld repairs produced improved remaining lives when compared to the service-aged girth weldments. Since the two ex-service weldments that were utilized in weld repairs exhibited different stress rupture strengths to start with, the performance of temper bead and postweld heat-treated (PWHT) repair could not be compared directly. It was clear, however, that life extension periods exceeding 30 yr could be achieved by temperbead repairs, with improved toughness and with no loss of stress rupture ductility, tensile strength, or yield strength. The temperbead repair improved the toughness of the service-aged weldment, while the postweld heat-treated repair lowered the HAZ toughness.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titlePerformance of Repair Welds on Service-Aged 2-1/4Cr-1Mo Girth Weldments
dc.typeJournal Paper
dc.journal.volume119
dc.journal.issue4
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.2842324
dc.journal.fristpage414
dc.journal.lastpage422
dc.identifier.eissn1528-8978
dc.keywordsMaintenance
dc.keywordsWelded joints
dc.keywordsPipes
dc.keywordsToughness
dc.keywordsHeat
dc.keywordsRupture
dc.keywordsStress
dc.keywordsDuctility
dc.keywordsLife extension
dc.keywordsTensile strength
dc.keywordsMechanical testing
dc.keywordsPiping systems AND Yield strength
dc.treeJournal of Pressure Vessel Technology:;1997:;volume( 119 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record