    Fatigue Crack Growth Properties of a Cryogenic Structural Steel at Liquid Helium Temperature

    Thumbnail
    View/Open
    JEMTA8-26976#109_1.pdf (610.6Kb)
    Date
    1996
    Author
    Shinji Konosu
    Yoshihiko Nunoya
    Hideo Nakajima
    Tomohiro Kishiro
    Ogi Ivano
    Hiroshi Tsuji
    Metadata
    Show full item record
    Abstract
    The structural materials of the coils of superconducting magnets utilized in thermonuclear fusion reactors are used at liquid helium (4.2 K) temperatures and are subjected to repeated thermal stresses and electromagnetic forces. A high strength, high toughness austenitic stainless steel (12Cr-12Ni-10Mn-5Mo-0.2N) has recently been developed for large, thick-walled components used in such environments. This material is non-magnetic even when subjected to processing and, because it is a forging material, it is advantageous as a structural material for large components. In the current research, a large forging of 12Cr-12Ni-10Mn-5Mo-0.2N austenitic stainless steel, was fabricated to a thickness of 250 mm, which is typical of section thicknesses encountered in actual equipment. The tensile fatigue crack growth properties of the forging were examined at liquid helium temperature as function of specimen location across the thickness of the forging. There was virtually no evidence of variation in tensile strength or fatigue crack growth properties attributable to different sampling locations in the thickness direction and no effect of thickness due to the forging or solution treatment associated with large forgings was observed. It has been clarified that there are cases in which small scale yielding (SSY) conditions are not fulfilled when stress ratios are large. ΔJ was introduced in order to achieve unified expression inclusive of these regions and, by expressing crack growth rate accordingly, the following formula was obtained at the second stage (middle range). da/dN = CJ ΔJm J , CJ = AJ /(ΔJ0 )m J , where, AJ = 1.47 × 10−5 mm/cycle, ΔJ0 = 2.42 × 103 N/m.
    URI
    http://yetl.yabesh.ir/yetl/handle/yetl/117085
    Collections
    • Journal of Engineering Materials and Technology

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV
     

     

    Browse

    All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Statistics

    View Usage Statistics

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV