dc.description.abstractResults are presented on the interlaminar shear strength (ILSS) and Mode I fracture toughness (GIC ) of glass/epoxy laminates interleaved with thermoplastic polyester films using four-point bending and double cantilever beam tests, respectively. The ILSS equation from classical beam theory was modified to account for the increased film thickness. It was found that the ultimate failure load and ILSS could be doubled if a thermoplastic film of high ductility but low glass transition temperature is used. Good film/composite ply adhesion is necessary. Mode I fracture toughness is influenced by film thickness and interleaving with a 0.2 mm thick film increased the GIC by 40 percent. Interleaving with a thinner film (0.1 mm), however, resulted in adhesive failure and reduced fibre bridging.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleThe Influence of Thermoplastic Film Interleaving on the Interlaminar Shear Strength and Mode I Fracture of Laminated Composites
dc.typeJournal Paper
dc.journal.volume118
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.2806810
dc.journal.fristpage302
dc.journal.lastpage309
dc.identifier.eissn1528-8889
dc.keywordsComposite materials
dc.keywordsFracture (Process) AND Shear strength
dc.treeJournal of Engineering Materials and Technology:;1996:;volume( 118 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record