| dc.contributor.author | L. A. James | |
| dc.contributor.author | W. H. Cullen | |
| dc.contributor.author | G. L. Wire | |
| dc.date.accessioned | 2017-05-08T23:48:09Z | |
| dc.date.available | 2017-05-08T23:48:09Z | |
| dc.date.copyright | August, 1995 | |
| dc.date.issued | 1995 | |
| dc.identifier.issn | 0094-9930 | |
| dc.identifier.other | JPVTAS-28361#238_1.pdf | |
| dc.identifier.uri | http://yetl.yabesh.ir/yetl/handle/yetl/115847 | |
| dc.description.abstract | The effect of water flow rate upon the environmentally assisted cracking (EAC) response of a high-sulfur ferritic steel was studied at a temperature of 243°C. In contrast to earlier studies which employed compact-type specimens, this study employed relatively large tight semi-elliptical surface cracks tested under generally linear-elastic conditions. Flow velocities parallel to the crack as low as 1.58–1.84 m/s were effective in mitigating EAC. | |
| dc.publisher | The American Society of Mechanical Engineers (ASME) | |
| dc.title | The Effect of Water Flow Rate Upon the Environmentally Assisted Cracking Response of a Low-Alloy Steel | |
| dc.type | Journal Paper | |
| dc.journal.volume | 117 | |
| dc.journal.issue | 3 | |
| dc.journal.title | Journal of Pressure Vessel Technology | |
| dc.identifier.doi | 10.1115/1.2842117 | |
| dc.journal.fristpage | 238 | |
| dc.journal.lastpage | 244 | |
| dc.identifier.eissn | 1528-8978 | |
| dc.keywords | Flow (Dynamics) | |
| dc.keywords | Alloys | |
| dc.keywords | Steel | |
| dc.keywords | Fracture (Process) | |
| dc.keywords | Water | |
| dc.keywords | Sulfur | |
| dc.keywords | Surface cracks | |
| dc.keywords | Fracture (Materials) AND Temperature | |
| dc.tree | Journal of Pressure Vessel Technology:;1995:;volume( 117 ):;issue: 003 | |
| dc.contenttype | Fulltext | |