dc.description.abstractWeight functions for the surface and the deepest point of an internal longitudinal semi-elliptical crack in a thick-wall cylinder (Ri /t = 1) were derived from a general weight function and two reference stress intensity factors. For several linear and nonlinear crack face stress, fields, the weight functions were validated against finite element data. Stress intensity factors were also calculated for the Lamé through the thickness stress distribution induced by internal pressure. The weight functions appear to be particularly suitable for fatigue and fracture analysis of surface semi-elliptical cracks in complex stress fields. All stress intensity factor expressions given in the paper are valid for cylinders with the inner-radius-to-wall-thickness ratio, Ri /t = 1.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleWeight Functions and Stress Intensity Factors for Longitudinal Semi-Elliptical Cracks in Thick-Wall Cylinders
dc.typeJournal Paper
dc.journal.volume117
dc.journal.issue4
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.2842140
dc.journal.fristpage383
dc.journal.lastpage389
dc.identifier.eissn1528-8978
dc.keywordsWeight (Mass)
dc.keywordsStress
dc.keywordsFracture (Materials)
dc.keywordsCylinders
dc.keywordsFunctions
dc.keywordsThickness
dc.keywordsFinite element analysis
dc.keywordsFracture (Process)
dc.keywordsStress concentration
dc.keywordsPressure AND Fatigue
dc.treeJournal of Pressure Vessel Technology:;1995:;volume( 117 ):;issue: 004
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record