dc.description.abstractFracture Toughness of HIP-sintered silicon nitride decreased with increasing temperature up to 1200°C. The brittle-to-ductile transition was observed in the temperature range from 1200°C to 1275°C: the fracture toughness rapidly increased in the transition region. Above the transition temperature, the fracture toughness decreased with increasing temperature. Fracture toughness of sialon increased with increasing temperature. Transition of fracture mechanism was observed in sialon around 1300°C. The differences of temperature dependence of fracture toughness between two materials are interpreted in terms of the effects of grain-boundary glass phase on fracture.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleHigh Temperature Fracture Toughness in Silicon Nitride and Sialon
dc.typeJournal Paper
dc.journal.volume115
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.2904217
dc.journal.fristpage268
dc.journal.lastpage272
dc.identifier.eissn1528-8889
dc.keywordsSilicon nitride ceramics
dc.keywordsFracture toughness
dc.keywordsHigh temperature
dc.keywordsTemperature
dc.keywordsFracture (Process)
dc.keywordsGlass
dc.keywordsBrittleness
dc.keywordsGrain boundaries
dc.keywordsMechanisms AND Phase transition temperature
dc.treeJournal of Engineering Materials and Technology:;1993:;volume( 115 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record