| dc.contributor.author | J. A. Todd | |
| dc.contributor.author | J. C. Ren | |
| dc.date.accessioned | 2017-05-08T23:39:21Z | |
| dc.date.available | 2017-05-08T23:39:21Z | |
| dc.date.copyright | August, 1992 | |
| dc.date.issued | 1992 | |
| dc.identifier.issn | 0094-9930 | |
| dc.identifier.other | JPVTAS-28337#364_1.pdf | |
| dc.identifier.uri | http://yetl.yabesh.ir/yetl/handle/yetl/110756 | |
| dc.description.abstract | The MC precipitate size distributions have been measured for times of 1, 10, 100, 300 and 1000 hr at 700 and 900° C in a 16Ni-14Cr advanced austenitic steel. A new correlation between the mean precipitate size, aging time and temperature has been developed. The new correlation is compatible with a solute exhaustion mechanism, which may explain why (i) the MC precipitates formed on matrix dislocations resist coarsening for up to 3000 hr at 900°C; and (ii) the degree of cold work (i.e., the dislocation density), which determines the number of MC nucleation sites, controls the limiting precipitate size. | |
| dc.publisher | The American Society of Mechanical Engineers (ASME) | |
| dc.title | A New Correlation Between MC Precipitate Size, Aging Time and Temperature for an Advanced Austenitic Steel | |
| dc.type | Journal Paper | |
| dc.journal.volume | 114 | |
| dc.journal.issue | 3 | |
| dc.journal.title | Journal of Pressure Vessel Technology | |
| dc.identifier.doi | 10.1115/1.2929053 | |
| dc.journal.fristpage | 364 | |
| dc.journal.lastpage | 368 | |
| dc.identifier.eissn | 1528-8978 | |
| dc.keywords | Temperature | |
| dc.keywords | Steel | |
| dc.keywords | Nucleation (Physics) | |
| dc.keywords | Dislocation density | |
| dc.keywords | Dislocations AND Mechanisms | |
| dc.tree | Journal of Pressure Vessel Technology:;1992:;volume( 114 ):;issue: 003 | |
| dc.contenttype | Fulltext | |