dc.contributor.authorS. K. Mukherjee
dc.contributor.authorV. Chexal
dc.contributor.authorN. A. Goldstein
dc.contributor.authorB. F. Beaudoin
dc.contributor.authorD. F. Quiñones
dc.contributor.authorD. M. Norris
dc.contributor.authorJ. J. Szy Slow Ski
dc.contributor.authorW. L. Server
dc.date.accessioned2017-05-08T23:30:55Z
dc.date.available2017-05-08T23:30:55Z
dc.date.copyrightFebruary, 1989
dc.date.issued1989
dc.identifier.issn0094-9930
dc.identifier.otherJPVTAS-28307#64_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/105916
dc.description.abstractFor much of the high-energy piping in light water reactor systems, fracture mechanics calculations can be used to assure pipe failure resistance, thus allowing the elimination of excessive rupture restraint hardware both inside and outside containment. These calculations use the concept of leak-before-break (LBB) and include part-through-wall flaw fatigue crack propagation, through-wall flaw detectable leakage, and through-wall flaw stability analyses. Performing these analyses not only reduces initial construction, future maintenance, and radiation exposure costs, but also improves the overall safety and integrity of the plant since much more is known about the piping and its capabilities than would be the case had the analyses not been performed. This paper presents the LBB methodology applied at Beaver Valley Power Station—Unit 2 (BVPS-2); the application for two specific lines, one inside containment (stainless steel) and the other outside containment (ferritic steel), is shown in a generic sense using a simple parametric matrix. The overall results for BVPS-2 indicate that pipe rupture hardware is not necessary for stainless steel lines inside containment greater than or equal to 6-in. (152-mm) nominal pipe size that have passed a screening criteria designed to eliminate potential problem systems (such as the feedwater system). Similarly, some ferritic steel line as small as 3-in. (76-mm) diameter (outside containment) can qualify for pipe rupture hardware elimination.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleRupture Hardware Minimization in Pressurized Water Reactor Piping
dc.typeJournal Paper
dc.journal.volume111
dc.journal.issue1
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3265641
dc.journal.fristpage64
dc.journal.lastpage71
dc.identifier.eissn1528-8978
dc.keywordsHardware
dc.keywordsPipes
dc.keywordsRupture
dc.keywordsPressurized water reactors
dc.keywordsContainment
dc.keywordsStainless steel
dc.keywordsSteel
dc.keywordsMaintenance
dc.keywordsRadiation (Physics)
dc.keywordsSafety
dc.keywordsElectrical resistance
dc.keywordsConstruction
dc.keywordsFeedwater
dc.keywordsStability
dc.keywordsFracture mechanics
dc.keywordsLeakage
dc.keywordsLight water reactors
dc.keywordsPower stations
dc.keywordsFailure
dc.keywordsFatigue cracks
dc.keywordsIndustrial plants
dc.keywordsPipe sizes AND Leak-before-break
dc.treeJournal of Pressure Vessel Technology:;1989:;volume( 111 ):;issue: 001