dc.description.abstractRealistic fired heater tube-life predictions are essential to safe and economical design, proactive inspection strategy and meaningful tube retirement evaluations. The traditional method of heater tube design (API RP 530), that is based on the “mean-diameter equation,” sometimes implies tube-life in excess of actual operating experience. The main reason for this discrepancy is the interaction of cyclic radial thermal gradient, that exists across the tube wall, with the pressure-induced stresses resulting in enhanced creep damage. Upper-bound estimates for creep deformations and creep damage are obtained in this paper using a simple analytical procedure. Some broad guidelines relating to the assessment of remaining tube-life, tube retirement and inspection frequencies are presented.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleDesign and Life Prediction of Fired Heater Tubes in the Creep Range
dc.typeJournal Paper
dc.journal.volume110
dc.journal.issue3
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3265606
dc.journal.fristpage322
dc.journal.lastpage328
dc.identifier.eissn1528-8978
dc.keywordsCreep
dc.keywordsDesign
dc.keywordsInspection
dc.keywordsStress
dc.keywordsPressure
dc.keywordsDeformation
dc.keywordsEquations
dc.keywordsFrequency
dc.keywordsAmerican Petroleum Institute AND Temperature gradients
dc.treeJournal of Pressure Vessel Technology:;1988:;volume( 110 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record