dc.description.abstractStandard fatigue precracking of fracture toughness specimens taken from stainless steel welds with a double-V design was found to result in extremely uneven crack fronts. Material variability within the weld zone could not explain the irregular crack fronts, which must therefore be associated with residual stress effects. Uniform fatigue cracks could be obtained by sectioning the double-V weld at the mid-thickness to relieve residual stresses and by precracking at a stress ratio of 0.4. Residual stresses can impact the leak-before-break position for welded structures.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleResidual Stress Effects on Fatigue Crack Growth Behavior in Stainless Steel Welds
dc.typeJournal Paper
dc.journal.volume109
dc.journal.issue3
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3264874
dc.journal.fristpage336
dc.journal.lastpage339
dc.identifier.eissn1528-8978
dc.keywordsStress
dc.keywordsWelded joints
dc.keywordsFatigue cracks
dc.keywordsStainless steel
dc.keywordsResidual stresses
dc.keywordsFracture (Materials)
dc.keywordsDesign
dc.keywordsFatigue
dc.keywordsFracture toughness
dc.keywordsThickness AND Leak-before-break
dc.treeJournal of Pressure Vessel Technology:;1987:;volume( 109 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record