dc.contributor.authorD. Green
dc.contributor.authorR. Parker
dc.contributor.authorD. Marsh
dc.date.accessioned2017-05-08T23:25:29Z
dc.date.available2017-05-08T23:25:29Z
dc.date.copyrightNovember, 1987
dc.date.issued1987
dc.identifier.issn0094-9930
dc.identifier.otherJPVTAS-28294#421_1.pdf
dc.identifier.urihttp://yetl.yabesh.ir/yetl/handle/yetl/102880
dc.description.abstractThis paper reports the theoretical assessment of cracking which may occur when a severe cycle comprising alternate upshocks and downshocks is applied to an axisymmetric feature with an internal, partial penetration weld and crevice. The experimental observations of cracking are reported separately. A good agreement was noted even though extensive cycle plasticity occurred at the location of cracking. It is concluded that the LEFM solution has correlated with the experiment mainly because of the axisymmetric geometry which allows a large hydrostatic stress to exist at the internal weld crevice end. Thus the stress at the crevice can approach the singular solution required for LEFM correlations without contributing to yielding.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleComparison of Theoretical Estimates and Experimental Measurements of Fatigue Crack Growth Under Severe Thermal Shock Conditions—Part II: Theoretical Assessment and Comparison With Experiment
dc.typeJournal Paper
dc.journal.volume109
dc.journal.issue4
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3264925
dc.journal.fristpage421
dc.journal.lastpage427
dc.identifier.eissn1528-8978
dc.keywordsHydrostatics
dc.keywordsPlasticity
dc.keywordsMeasurement
dc.keywordsStress
dc.keywordsFracture (Process)
dc.keywordsCycles
dc.keywordsFatigue cracks
dc.keywordsGeometry AND Thermal shock
dc.treeJournal of Pressure Vessel Technology:;1987:;volume( 109 ):;issue: 004