dc.description.abstractA method of directly measuring the temperature rise during high speed torsion tests is described. The test sample is formed by welding two materials of similar mechanical properties but different thermoelectric characteristics and ensuring, by reducing the section, that the gauge length includes the thermocouple junction. A number of tests were conducted using the nickel base thermocouple alloys Nicrosil and Nisil (I.S.A. Type N). The temperature rise observed during uniform deformation agrees with that expected from simple thermomechanical calculations. Void growth and coalescence lead to a strain concentration and ductile fracture which is accompanied by a more significant temperature rise.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleDirect Measurement of Temperature in High Speed Torsion Tests
dc.typeJournal Paper
dc.journal.volume109
dc.journal.issue2
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225953
dc.journal.fristpage140
dc.journal.lastpage145
dc.identifier.eissn1528-8889
dc.keywordsTemperature measurement
dc.keywordsTorsion
dc.keywordsTemperature
dc.keywordsThermocouples
dc.keywordsDuctile fracture
dc.keywordsDeformation
dc.keywordsNickel
dc.keywordsAlloys
dc.keywordsGages
dc.keywordsMechanical properties
dc.keywordsJunctions AND Welding
dc.treeJournal of Engineering Materials and Technology:;1987:;volume( 109 ):;issue: 002