dc.description.abstractTest specimens were cut from a 25-mm-thick Type 316 stainless steel plate butt welded with 16-8-2 filler wire. The specimens were oriented transverse to the weld seam and contained base metal, heat-affected zone (HAZ), and weld metal in the gage section. Strain-controlled cyclic loading at room temperature was imposed across the heterogeneous weldment while local strains at various points within the gage section were continuously monitored. Results show that strains at the local points can vary markedly from the average strain of the composite section. Strain concentrations occurred in the softer base metal which led to failure much sooner than the composite strain would indicate. However, when the maximum strain range from a local area was compared to baseline data, the life correlation was very good.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleStrain Distributions in a Type 316/16-8-2 Stainless Steel Weldment During Cyclic Loading
dc.typeJournal Paper
dc.journal.volume108
dc.journal.issue1
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3264745
dc.journal.fristpage120
dc.journal.lastpage123
dc.identifier.eissn1528-8978
dc.keywordsStainless steel
dc.keywordsComposite materials
dc.keywordsGages
dc.keywordsBase metals
dc.keywordsFailure
dc.keywordsHeat
dc.keywordsTemperature
dc.keywordsMetals
dc.keywordsWire AND Fillers (Materials)
dc.treeJournal of Pressure Vessel Technology:;1986:;volume( 108 ):;issue: 001
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record