dc.description.abstractStress redistributions during local Post Weld Heat Treatments (PWHT) are numerically studied for a multi-pass butt-welded pipe with mechanically unrestrained ends. The pipe material is a micro-alloyed C-Mn steel. Temperature and stress fields developed during welding and PWHT are determined from a FE-analysis where rotational symmetry is assumed. Use of heaters with a total axial width less than four times the pipe wall thickness is found to result in substantially different final stress fields than those obtained after a uniform (furnace) heat treatment. The tensile axial and hoop stresses on the inner pipe surface near the centre section of the weldment are considerably higher after a local PWHT. The differences were found to arise mainly during the cooling periods of the PWHTs.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleStress Redistribution During Local Annealing of a Multi-Pass Butt-Welded Pipe
dc.typeJournal Paper
dc.journal.volume108
dc.journal.issue2
dc.journal.titleJournal of Pressure Vessel Technology
dc.identifier.doi10.1115/1.3264759
dc.journal.fristpage125
dc.journal.lastpage130
dc.identifier.eissn1528-8978
dc.keywordsAnnealing
dc.keywordsStress
dc.keywordsPipes
dc.keywordsFurnaces
dc.keywordsWall thickness
dc.keywordsHeat treating (Metalworking)
dc.keywordsFinite element analysis
dc.keywordsHeat
dc.keywordsTemperature
dc.keywordsCooling
dc.keywordsSteel AND Welding
dc.treeJournal of Pressure Vessel Technology:;1986:;volume( 108 ):;issue: 002
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record