dc.description.abstractThe coefficient of thermal expansion (CTE) of a hot pressed Ta16 W18 O94 which was produced from Ta2 O5 and WO3 powders was found to be −1.52×10−6 K−1 in the temperature range 180–330 K. Using the Ta16 W18 O94 and Super Invar powders, 50:50 volume percent metal-ceramic composites were made by the powder metallurgy techniques. When the mixture of constituent powders was hot pressed at 1123 K for 10 minutes, a CTE of 1.1 × 10−6 K−1 was obtained in the temperature range 140–420 K.
dc.publisherThe American Society of Mechanical Engineers (ASME)
dc.titleThe Coefficient of Thermal Expansion of a Super Invar-Ta16W18O94 Composite
dc.typeJournal Paper
dc.journal.volume108
dc.journal.issue3
dc.journal.titleJournal of Engineering Materials and Technology
dc.identifier.doi10.1115/1.3225880
dc.journal.fristpage270
dc.journal.lastpage274
dc.identifier.eissn1528-8889
dc.keywordsThermal expansion
dc.keywordsComposite materials
dc.keywordsInvar
dc.keywordsTemperature
dc.keywordsCermets
dc.keywordsPowder metallurgy AND Mixtures
dc.treeJournal of Engineering Materials and Technology:;1986:;volume( 108 ):;issue: 003
dc.contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record