Residual Stress Analysis by Simplified Inherent Strain at Welded Pipe Junctures in a Pressure Vessel
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: We present a new and simplified method of estimating residual stress in welded structures by using inherent strain. The method makes use of elastic analysis by means of the finite element ...
Vibration Behavior and Fatigue Strength of Mocked-Up Piping System
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: For the purpose of investigating vibration characteristics and fatigue strength of a socket-welded joint, a piping system was mocked-up by assembling a straight pipe of 350 mm nominal diameter ...
Characteristics of Homogeneous Charge Compression Ignition (HCCI) Engine Operation for Variations in Compression Ratio, Speed, and Intake Temperature While Using n-Butane as a Fuel
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: In this paper, some basic properties of homogeneous charge compression ignition operation are reported. The effect of inlet temperature, compression ratio and engine speed on the homogeneous ...
Residual Stresses in Steel and Zirconium Weldments
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: Three-dimensional scans of residual stress within intact weldments provide insight into the consequences of various welding techniques and stress-relieving procedures. The neutron diffraction method ...
Analytical Study on Fatigue Strength Reduction Factor of Small-Diameter Socket-Welded Pipe Joints
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: Four-point bending and rotating bending fatigue tests were conducted on socket-welded joints made of carbon, stainless, and Cr-Mo steels for clarification of the effects of diameter, welding pass ...
Experimental Study on Fatigue Strength of Small-Diameter Socket-Welded Pipe Joints
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: The authors conducted fully reversed four-point bending fatigue tests on socket-welded joints 20 to 50 mm in nominal diameter, and rotating bending fatigue tests on socket-welded joints 20 mm ...