Search
Now showing items 1-6 of 6
Effects of Residual Stress on Fatigue Strength of Small-Diameter Welded Pipe Joint
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: Bending fatigue tests were conducted to investigate the fatigue strength of small-diameter socket welded pipe joints. In most cases of large-diameter socket joints, a fatigue crack started from ...
Vibration Behavior and Fatigue Strength of Mocked-Up Piping System
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: For the purpose of investigating vibration characteristics and fatigue strength of a socket-welded joint, a piping system was mocked-up by assembling a straight pipe of 350 mm nominal diameter ...
Effects of Crack Starter Bead Preparation in Drop-Weight Test on Nil-Ductility Transition Temperature
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: The procedure for making crack starter weld deposit on drop-weight test (DWT) specimens was altered from two passes to one pass in about 1990. The effects of some parameters of crack starter ...
Fatigue Crack Growth Curve for Austenitic Stainless Steels in BWR Environment
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: Fatigue crack growth data obtained in the simulated BWR water environment were analyzed to establish a formula for reference fatigue crack growth rate (FCGR) of austenitic stainless steels in ...
Analytical Study on Fatigue Strength Reduction Factor of Small-Diameter Socket-Welded Pipe Joints
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: Four-point bending and rotating bending fatigue tests were conducted on socket-welded joints made of carbon, stainless, and Cr-Mo steels for clarification of the effects of diameter, welding pass ...
Experimental Study on Fatigue Strength of Small-Diameter Socket-Welded Pipe Joints
Publisher: The American Society of Mechanical Engineers (ASME)
Abstract: The authors conducted fully reversed four-point bending fatigue tests on socket-welded joints 20 to 50 mm in nominal diameter, and rotating bending fatigue tests on socket-welded joints 20 mm ...