description abstractIn this paper, setting time, strength and bond of high-calcium fly ash geopolymer concrete were investigated. The high-calcium fly ash was from Mae Moh power plant in northern Thailand. Both sodium silicate solution and sodium hydroxide solution were used as alkali activators in every mix. Sodium hydroxide solution with 10 M, 15 M, and 20 M concentrations, sodium silicate to sodium hydroxide ratios of 1.0 and 2.0, alkaline liquid to fly ash ratio of 0.5 and two curing regimes viz., heat curing at
publisherAmerican Society of Civil Engineers
titleSetting Time, Strength, and Bond of High-Calcium Fly Ash Geopolymer Concrete
typeJournal Paper
journal volume27
journal issue7
journal titleJournal of Materials in Civil Engineering
identifier doi10.1061/(ASCE)MT.1943-5533.0001157
treeJournal of Materials in Civil Engineering:;2015:;Volume ( 027 ):;issue: 007
contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record