description abstractThe fatigue performance of concrete bridge decks with glass fiber–reinforced polymer (GFRP) stay-in-place structural forms replacing the bottom layer of rebar is studied. The forms were either flat plate with T-up ribs joined using lap splices or corrugated forms joined through pin-and-eye connections. The decks were supported by simulated precast girders, AASHTO Type III, spaced at 1,775 mm. Two surface preparations were examined for each GFRP form, either using adhesive coating that bonds to freshly cast concrete, or just cleaning the surface before casting. For the bonded deck with flat-ribbed forms, adhesive bond and mechanical fasteners were used at the lap splice, whereas lap splice of the unbonded deck had no adhesive or mechanical fasteners. All decks survived 3 million cycles at 123 kN service load of the CL625 design truck of the Canadian standard. The bonded flat-ribbed-form deck further survived additional 2 million cycles at a higher load simulating a larger girder spacing of 2,365 mm. Stiffness degradations were 9–33% with more reduction in unbonded specimens. Nonetheless, live load deflections of all specimens remained below
publisherAmerican Society of Civil Engineers
titleFatigue Behavior of Concrete Bridge Decks Cast on GFRP Stay-in-Place Structural Forms
typeJournal Paper
journal volume18
journal issue3
journal titleJournal of Composites for Construction
identifier doi10.1061/(ASCE)CC.1943-5614.0000432
treeJournal of Composites for Construction:;2014:;Volume ( 018 ):;issue: 003
contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record