contributor authorC. E. Jaske
contributor authorH. Mindlin
contributor authorJ. S. Perrin
date accessioned2017-05-09T01:35:09Z
date available2017-05-09T01:35:09Z
date copyrightAugust, 1972
date issued1972
identifier issn1087-1357
identifier otherJMSEFK-27575#930_1.pdf
identifier urihttp://yetl.yabesh.ir/yetl/handle/yetl/163093
description abstractA study has been conducted to determine the low-cycle fatigue behavior of solution-annealed Incoloy 800 bar at temperatures from 800–1400 deg F. The experimental work included evaluation of specimens under both continuous, completely reversed strain cycling and under strain cycling with hold time periods at the strain limits. At 1000, 1200, and 1400 deg F, it was found that 10-min hold-times at the tensile strain limit during every cycle significantly reduced the cyclic fatigue life compared to continuous cycling. However, there was little reduction in cyclic fatigue life when 10-min hold-times were introduced at the compressive strain limits or at both the tensile and compressive limits. The ratio of hold-time cyclic fatigue life to no-hold-time cyclic fatigue life decreased as the length of hold time increased (at constant total strain range) and as the magnitude of strain range decreased (at constant hold-time length).
publisherThe American Society of Mechanical Engineers (ASME)
titleInfluence of Hold-Time and Temperature on the Low-Cycle Fatigue of Incoloy 800
typeJournal Paper
journal volume94
journal issue3
journal titleJournal of Manufacturing Science and Engineering
identifier doi10.1115/1.3428273
journal fristpage930
journal lastpage934
identifier eissn1528-8935
keywordsTemperature
keywordsLow cycle fatigue
keywordsFatigue life AND Cycles
treeJournal of Manufacturing Science and Engineering:;1972:;volume( 094 ):;issue: 003