Show simple item record

contributor authorCohn, Marvin J.
contributor authorFaham, Fatma G.
contributor authorPatel, Dipak
date accessioned2017-05-09T01:32:53Z
date available2017-05-09T01:32:53Z
date issued2016
identifier issn0094-9930
identifier otherht_138_07_074503.pdf
identifier urihttp://yetl.yabesh.ir/yetl/handle/yetl/162404
description abstractA highenergy piping (HEP) asset integrity management program is important for the safety of plant personnel and reliability of the fossil plant generating unit. HEP weldment failures have resulted in serious injuries, fatalities, extensive damage of components, and significant lost generation. The main steam (MS) piping system is one of the most critical HEP systems. Creep damage assessment in MS piping systems should include the evaluation of multiaxial stresses associated with field conditions and significant anomalies, such as malfunctioning supports and significant displacement interferences. This paper presents empirical data illustrating that the most critical girth welds of MS piping systems have creep failures which can be successfully ranked by a multiaxial stress parameter, such as maximum principal stress. Inelastic (redistributed) stresses at the piping outside diameter (OD) surface were evaluated for the base metal of three MS piping systems at the piping analysis model nodes. The range of piping system stresses at the piping nodes for each piping system was determined for the redistributed creep stress condition. The range of piping stresses was subsequently included on a Larson–Miller parameter (LMP) plot for the grade P22 material, revealing the few critical (leadthefleet) girth welds selected for nondestructive examination (NDE). In the three MS piping systems, the stress ranges varied from 55% to 80%, with only a few locations at stresses beyond the 65 percentile of the range. By including evaluations of significant field anomalies and the redistributed multiaxial stresses on the outside surface, it was shown that there is a good correlation of the ranked redistributed multiaxial stresses to the observed creep damage. This process also revealed that a large number of MS piping girth welds have insufficient applied stresses to develop substantial creep damage within the expected unit lifetime (assuming no major fabrication defects). This study also provided a comparison of the results of a conventional American Society of Mechanical Engineers (ASME) B31.1 Code asdesigned sustained stress analysis versus the redistributed maximum principal stresses in the asfound (current) condition for a complete set of MS piping system nodes. The evaluations of redistributed maximum principal stresses in the asfound condition were useful in selecting high priority ranked girth weldment creep damage locations. The evaluations of B31.1 Code asdesigned sustained load stresses were not useful in selecting high priority creep damage locations.
publisherThe American Society of Mechanical Engineers (ASME)
titleRanking of Creep Damage in Main Steam Piping System Girth Welds Considering Multiaxial Stress Ranges
typeJournal Paper
journal volume138
journal issue4
journal titleJournal of Pressure Vessel Technology
identifier doi10.1115/1.4033077
journal fristpage41202
journal lastpage41202
identifier eissn1528-8978
treeJournal of Pressure Vessel Technology:;2016:;volume( 138 ):;issue: 004