description abstractAn innovative manufacturing method, bladder assisted composite manufacturing (BACM), to fabricate geometrically complex, hollow parts made of polymeric composite materials is presented. Unlike the conventional bladder or diaphragm assisted curing processes, BACM uses an internally heated bladder to provide the consolidation pressure at the required cure temperature. The feasibility of this manufacturing method is demonstrated by fabricating laminated composite cylinders using multiple cure pressures and number of plies. The elastic moduli, failure strength, fiber volume fraction, and void contents of the cylinders were found to be comparable to the values obtained from flat laminates produced by hot plate molding of the same material. Compared to conventional bladder manufacturing methods, the BACM process reduced the energy required to cure the cylinders by almost 50% due to internal heating and insulated mold.
publisherThe American Society of Mechanical Engineers (ASME)
titleProperties of Composite Cylinders Fabricated by Bladder Assisted Composite Manufacturing
typeJournal Paper
journal volume134
journal issue4
journal titleJournal of Engineering Materials and Technology
identifier doi10.1115/1.4007017
journal fristpage44501
identifier eissn1528-8889
keywordsPressure
keywordsComposite materials
keywordsFibers
keywordsLaminates
keywordsManufacturing
keywordsCylinders
keywordsHeating AND Curing
treeJournal of Engineering Materials and Technology:;2012:;volume( 134 ):;issue: 004
contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record