Show simple item record

contributor authorHyeong-Yeon Lee
contributor authorKee-Nam Song
contributor authorYong-Wan Kim
date accessioned2017-05-09T00:40:33Z
date available2017-05-09T00:40:33Z
date copyrightJune, 2010
date issued2010
identifier issn0094-9930
identifier otherJPVTAS-28533#031101_1.pdf
identifier urihttp://yetl.yabesh.ir/yetl/handle/yetl/144679
description abstractEvaluation of creep-fatigue damage has been carried out for the hot gas duct (HGD) structure in the nuclear hydrogen development and demonstration (NHDD) plant. The core outlet and inlet temperature of the NHDD plant are 950°C and 490°C, respectively. Case studies on high temperature design codes of the draft code case for Alloy 617, ASME boiler and pressure vessel code section III subsection NH (ASME-NH), and RCC-MR were carried out for the inner tube of the HGD for the candidate materials of Alloy 617 and Alloy 800H. Technical issues in application of the draft code case to a high temperature structure are discussed for the Alloy 617 material. Code comparison between the ASME-NH and RCC-MR for Alloy 800H has been carried out. The candidate material of the outer pressure boundary (cross vessel) of the HGD is Mod.9Cr-1Mo steel. The damage evaluation, according to the ASME-NH and RCC-MR for the cross vessel of Mod.9Cr-1Mo steel, has been conducted and their results were compared.
publisherThe American Society of Mechanical Engineers (ASME)
titleEvaluation of Creep-Fatigue Damage for Hot Gas Duct Structure of the NHDD Plant
typeJournal Paper
journal volume132
journal issue3
journal titleJournal of Pressure Vessel Technology
identifier doi10.1115/1.4000728
journal fristpage31101
identifier eissn1528-8978
keywordsCreep
keywordsFatigue
keywordsAlloys
keywordsVessels
keywordsDesign
keywordsDucts AND Industrial plants
treeJournal of Pressure Vessel Technology:;2010:;volume( 132 ):;issue: 003