Show simple item record

contributor authorJ. F. Warriner
contributor authorD. L. Westerling
date accessioned2017-05-08T23:35:27Z
date available2017-05-08T23:35:27Z
date copyrightJuly, 1991
date issued1991
identifier issn1528-8919
identifier otherJETPEZ-26689#331_1.pdf
identifier urihttp://yetl.yabesh.ir/yetl/handle/yetl/108509
description abstractAfter a brief history of the introduction of galvanically applied overlays to the surface of thin-walled half-bearings, the paper goes on to describe experiences in service engines. This shows that from the mid-1970s, overlay life could be sharply reduced due to a variety (or combination) of factors. These are described, the possible causes explained, and various palliatives investigated. The principle factor in the mid-1970s was the rapid rise in the use of lower quality heavy fuels initiated by escalating oil costs. The consequence of using these fuels was often rapid overlay loss, which in turn resulted in further problems, particularly: large areas of exposed nickel interlay, corrosion of the overlay, and/or corrosion of the base lining material. Four palliatives, elimination of the overlay, harder overlays, elimination of the interlayer, and modified surface topography are described and results of development testing and field service experience are presented.
publisherThe American Society of Mechanical Engineers (ASME)
titleMedium-Speed Engine Bearings—Development Experience
typeJournal Paper
journal volume113
journal issue3
journal titleJournal of Engineering for Gas Turbines and Power
identifier doi10.1115/1.2906234
journal fristpage331
journal lastpage339
identifier eissn0742-4795
keywordsEngines
keywordsBearings
keywordsOverlays (Materials engineering)
keywordsFuels
keywordsCorrosion
keywordsTesting
keywordsNickel AND Linings (Textiles)
treeJournal of Engineering for Gas Turbines and Power:;1991:;volume( 113 ):;issue: 003
contenttypeFulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record